Achieve™ Advanced PP6282NE2 1.8 (230°C/2.16 kg)
Achieve™ Advanced PP3684 14 (230°C/2.16 kg)
Achieve™ Advanced PP3854 24 (230°C/2.16 kg)
Achieve™ Advanced PP8285E1 30 (230°C/2.16 kg)
Achieve™ Advanced PP1605 32 (230°C/2.16 kg)
Achieve™ Advanced PP7925E1 135 (230°C/2.16 kg)
Achieve™ Advanced PP6035G1 500 (230°C/2.16 kg)
Achieve™ Advanced PP6945G1 925 (230°C/2.16 kg)
Achieve™ Advanced PP6936G2 1550 (230°C/2.16 kg)